Microstructural and fractographic investigation of hydrogen embrittlement sensitivity of X70 pipeline steels

Published in 3rd Benelux Network Meeting and Workshop on Damage and Fracture Mechanics (BDFM-2023), Antwerp, Belgium, 2023

Download Poster (PDF)

Publication Link

Recommended citation: J. Jubica et al., "Microstructural and fractographic investigation of hydrogen embrittlement sensitivity of X70 pipeline steels," in 3rd Benelux Network Meeting and Workshop on Damage and Fracture Mechanics (BDFM-2023), Abstracts, Antwerp, Belgium, 2023.