Fractographic study for screening the hydrogen compatibility of X70 pipeline steels and welds
Published in IHC2023 : International Hydrogen Conference, Park City, Utah, USA, 2023
Link to the poster & publication
Recommended citation: L. Claeys et al., "Fractographic study for screening the hydrogen compatibility of X70 pipeline steels and welds," in IHC2023 : International Hydrogen Conference, Abstracts, Park City, Utah, USA, 2023.